| Item | Film faced plywood, Construction plywood, Form-work plywood |
| Film | Brown film, Black film, Red film, green PP plasctic,Anti-slip film, with logo |
| Core | Poplar, hardwood, combi, finger-joint core |
| Hot press | 1 time or 2 times |
| Glue | melamine WBP, phenolic WBP |
| Size | 1220×2440mm,1250×2500mm or as requirement |
| Thickness | 9mm, 12mm,15mm, 16.5mm, 17mm, 17.5mm, 18mm |
| Thickness tolerance | +/- 0.5mm |
| Density | 500-600 KGS/CBM |
| Moisture | To be 6%-14% at time of shipment |
| Usage | Construction, form-work |